In SX Microcontrollers, SX/B Compiler and SX-Key Tool, Coriolis wrote: You are correct ChrisP that an experienced developer can use mildly acidic flux and actually get better results when doing mass production. But unless you know what you are doing you should always stay away from acid based products when working with electronics, the potential downside is much worse than the potential upside. For a novice its best to stick with no-clean or water-clean fluxes. ---------- End of Message ---------- You can view the post on-line at: http://forums.parallax.com/forums/default.aspx?f=7&p=1&m=86586#m91599 Need assistance? Send an email to the Forum Administrator at forumadmin@parallax.com The Parallax Forums are powered by dotNetBB Forums, copyright 2002-2005 (http://www.dotNetBB.com)