Tal wrote: > I am using UV sensitive boards. > Please mention what developer you are using - for example=20 > I am using caustic soda (we call it like that I don't know > the real name) ... Sodium Carbonate Na2CO3. Didn't you think about not guessing, but rather just googling with your laminate name and "development" word? As example, for LAMINAR 5000 dry film this would be: ------------------- Table III - Developing Solution Temperature Breakpoint Sodium carbonate 0.75%-1.0% 28-33=B0C 50-60% Potassium carbonate 0.75%-1.0% 28-33=B0C 50-60% REsolve 211 0.75%- 1.0% 28-33=B0C 50-60% Developing time (sec) Laminar 5025 Laminar 5032 Laminar 5038 Laminar 5050 REsolve 211 30=B0C Breakpoint @ 50% 37 45 55 75 (4-ft chamber) ------------------- Good Luck. Mike. -- http://www.piclist.com hint: The PICList is archived three different ways. See http://www.piclist.com/#archives for details.