At 01:43 PM 3/27/02 -0500, you wrote: >There is a product used in setting flowers and the like. You mix two= portions >and pour it on your project. It will harden to a clear plastic. Check your= =20 >local >flower shop/gift shop for the product. >Rick > >Jay Hanson wrote: > > > I would like to encase a small circuit board in some sort of clear= plastic. > > Should I melt lexan, plexiglass, or ....? Is there is good liquid for= =20 > this? > > Fiberglass resin? > > > > What are the rest of you doing? The stuff they use for flowers is usually a polyester (activated resin + MEK as catalyst). Epoxies will handle a bit more heat but generally the tg= points are in the 150-250=B0F range (TG =3D transistion to Goo ;-]) I'd think the= =20 commercial conformal coating resins would be modified for a higher temp. Dave -- http://www.piclist.com hint: To leave the PICList mailto:piclist-unsubscribe-request@mitvma.mit.edu